The fireskin, and what strips it
The fireskin is the hard outer layer of a brick, the part closest to the heat of the kiln. The US Park Service explains what abrasive cleaning does to it: the hard layer is eroded, the soft inner core is left exposed to faster weathering, and the wall can take in more water than before (US National Park Service, 1979). The Irish guide to repairing historic brickwork says over-aggressive cleaning may remove the protective fireskin and leave the bricks open to accelerated decay (The Stationery Office, Dublin, 2009, pp. 43, 46).
Historic England's graffiti guidance shows the damage up close: scraping and abrasion have taken off the smooth, dark fireskin and exposed the lighter body underneath, and the streaks known in the trade as wand marks are typical of pressure washing (Historic England, 2021, pp. 11–12). The Irish guide warns that a great deal of brickwork has been damaged by compressed air and abrasives, and that jets of water are unnecessary and should not be used (The Stationery Office, Dublin, 2009, p. 45).
A laser is neither abrasive nor a water jet. That is why we put it first on brick, with the trial patch as the proof on each wall.
Which brick have you got?
Historic bricks range from soft, porous handmade bricks to much denser, harder machine-made ones (Historic England, 2021, p. 27). Traditionally made bricks can be more fragile than machine-made ones, and so easier to damage with the wrong materials and methods (The Stationery Office, Dublin, 2009, p. 4).
- Machine-made brick is rated for laser in the laser checker.
- Handmade or soft brick is rated , on trade practice rather than a cited document: soft brick varies from one brick to the next, so the energy starts low and rises slowly.
- Gauged brick, cut and rubbed to shape, is softer and more easily etched than other historic facing brick, and is often targeted by graffiti (Historic England, 2021, pp. 13–14). Treat it as the softest brick on the building.
- Glazed brick is damaged by strong acids and strong alkalis (US National Park Service, 1995), so any second step on it stays near neutral.
Doing it right on brick
- Trial first. The Irish guide calls a cleaning trial essential, specified, recorded and supervised, on an area truly typical of the wall (The Stationery Office, Dublin, 2009, p. 44).
- Start the energy low. Set too high, a laser can discolour or pit the surface (Historic England, 2021, p. 45).
- Pulsed, never continuous-wave. Historic England warns that longer pulses can leave a cracked, glassy layer on fired clay such as terracotta (Historic England, 2021, p. 45). See pulsed, not continuous-wave.
- Mind the joints. Mortar joints often behave differently from the bricks and typically prove harder to clean, and weak lime mortar responds differently again (Historic England, 2021, pp. 18, 31). Trial on a joint as well as a brick face.
- Run it safely. A cleaning laser is a Class 4 machine; see the law and the laser zone.
Practice note. Trial on the softest brick in the wall, not the best one. If the laser is safe on the weakest face, it is safe on the rest.
What finishes the job
Laser will not always take every trace alone. The 2023 laser trials left some residue even on the best results (npj Heritage Science, 2023), and Historic England says ghosting below the surface that needs a second treatment is quite usual (Historic England, 2021, p. 49).
- A poultice. The Irish guide suggests a suitable poultice for graffiti on historic brick (The Stationery Office, Dublin, 2009, p. 46), and the US Park Service calls it usually the most effective way to draw paint out of masonry without restaining it (US National Park Service, 1995).
- A gentle rinse. Heritage Victoria names steam and low-pressure hot water for heritage masonry (Heritage Victoria, 2022). The Irish guide keeps pre-wetting and rinsing historic brick at no higher than 400 psi (The Stationery Office, Dublin, 2009, p. 45); in the UK, low pressure is up to 17 bar, as Historic England reports the British Standard (Historic England, 2021, p. 37).
- Never caustic, never hydrofluoric. The US Park Service says caustic removers generally should not be used, because they can cause salt deposits and staining (US National Park Service, 1995), and the Irish guide calls products containing hydrofluoric acid highly corrosive (The Stationery Office, Dublin, 2009, p. 45).
And act quickly: the Irish guide says graffiti on historic brickwork should be cleaned off as soon as possible (The Stationery Office, Dublin, 2009, p. 46).