Hard stone, but not careless stone
Historic England describes granites as hard and impermeable, hard because their main mineral is quartz, and notes that robust surfaces such as granite are less vulnerable to damage from most cleaning methods (Historic England, 2021, pp. 27, 33–34). The US Park Service explains why graffiti often comes off polished granite comparatively easily: it is relatively impermeable, so the paint stays on the surface rather than soaking in (US National Park Service, 1995).
Hard does not mean safe from harsh treatment. Historic England warns that the polish of granite can be damaged by hard abrasives (Historic England, 2021, p. 33), and the US Park Service shows granite walls at the General Grant National Memorial in New York permanently damaged by harsh, and ineffective, graffiti removal (US National Park Service, 1995). A laser uses no abrasive, which is why it is the method to trial first.
What the laser trials on granite found
A 2018 study tested a Q-switched laser on blue, black and silver spray paint on a fine-grained granite (Coatings, 2018):
- Blue and black came off. They were removed most effectively when two laser wavelengths were used together.
- Silver did not. The aluminium-rich silver paint was not removed under any of the conditions tested.
- Paint in fissures stayed. The granite's natural cracks held paint where the beam could not reach it, and the binder in each paint made a large difference to how easily it came off.
- Too much energy damaged the stone. Above the stone's damage threshold, the dark mica, biotite, melted, and the stone's colour shifted.
A 2025 laboratory study on two other granites, made with a far shorter-pulsed laser than a site machine, found the same weak point: the micas were the first minerals to be damaged, then the feldspars, with quartz the last. Its authors conclude that settings have to be tailored case by case (Bulletin of Engineering Geology and the Environment, 2025).
Doing it right on granite
- Trial on each stone. Granites vary in their minerals and their fissures, and both decide the result (Coatings, 2018; Bulletin of Engineering Geology and the Environment, 2025). A trial on one block tells you about that block.
- Start the energy low and watch the dark grains. Mica melting or the stone changing colour is the sign to stop and turn down (Coatings, 2018).
- Pulsed, never continuous-wave. See pulsed, not continuous-wave.
- Run it safely. A cleaning laser is a Class 4 machine; see the law and the laser zone.
Practice note. Trial chrome and silver paint on its own patch. If the laser will not lift it at a safe setting, stop there and plan a different second step, rather than turning the energy up until the stone pays for it.
What finishes the job
Paint left in fissures, and silver paint, may need a second step. A poultice keeps a remover on the stain and draws it out without restaining the stone (US National Park Service, 1995), and Historic England says ghosting below the surface that needs a second treatment is quite usual (Historic England, 2021, p. 49). Choose the chemistry with care: the US Park Service lists some granites among the stones that alkalis can harm (US National Park Service, 1995). A rinse, where one is needed, stays at up to 17 bar (Historic England, 2021, p. 37).